3.9.4.3 Special Considerations for Joint Sealant
SBC 312 · Edition 2024 · p. 42
These are the clause's opening lines. The full clause, with its tables and exceptions, opens in the code reader.
Read the full clauseUnder this clause
- 3.9.4.3.1 Sealant failure cases for a joint shall be classified as adhesion failure or cohesion failure.
- 3.9.4.3.2 Adhesive failure cases occur when the sealant does not adhere well to the substrate.
- 3.9.4.3.3 Exposed surfaces are difficult to seal tightly; therefore, they shall be kept away from the faces of sealants.
- 3.9.4.3.4 Cohesive failure cases occur within the sealant material.
- 3.9.4.3.5 A common problem with sealant materials occurs in the substrate adjacent to the joint, particularly with silicone sealants; this problem is described in (Section 3.9.4.3.5).
- 3.9.4.3.6 Corner joints of precast concrete wall panels are considered among the difficult sealant details due to the movements that can occur at the corner joint.