13.2.1 Camber, Bowing, and Straightness

SBC 306 · Edition 2024 · p. 71

Thermal and mechanical means are permitted to be used to express or correct camber, bowing, and also out-of-straightness, provided that the temperature of the heated areas shall not exceed 590 °C for steels conforming to ASTM A514/A514M and ASTM A852/A852M,…

These are the clause's opening lines. The full clause, with its tables and exceptions, opens in the code reader.

Read the full clause